安全阀弹簧开裂原因分析

Fracture analysis for safety valve spring

  • 摘要: 对异常开裂失效的某电厂泵用安全阀弹簧的宏观形貌、化学成分、金相组织、微观形貌等进行了详细分析。结果表明:弹簧裂纹以沿晶脆性开裂特征为主,裂纹尖端尖锐,裂纹内有明显氧化,裂纹边缘无明显脱碳,为典型的淬火裂纹特征。

     

    Abstract: The reasons leading to fracture for the safety valve spring was analyzed by means of morphology analysis, mechanical properties test, hardness test, metallographic test and other detection means. The results show that the cracks of spring are mainly characterized by intergranular brittle cracking, with sharp crack tips, obvious oxidation inside the cracks, and no obvious decarburization at the crack edges, which are typical quenching crack characteristics.

     

/